{"_buckets": {"deposit": "dbe07d03-6baf-46a8-a9ef-3206bbd84570"}, "_deposit": {"created_by": 1, "id": "77224", "owners": [1], "pid": {"revision_id": 0, "type": "depid", "value": "77224"}, "status": "published"}, "_oai": {"id": "oai:repo.qst.go.jp:00077224", "sets": ["2"]}, "author_link": ["821823", "821815", "821822", "821817", "821821", "821818", "821816", "821819", "821820"], "item_10003_biblio_info_7": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2019-10", "bibliographicIssueDateType": "Issued"}, "bibliographicPageEnd": "711", "bibliographicPageStart": "709", "bibliographic_titles": [{"bibliographic_title": "Proceedings of the 16th Annual Meeting of Particle Accelerator Society of Japan"}]}]}, "item_10003_description_5": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "スポーク空洞は、周波数が同じならば楕円空洞よりサイズが小さく、さらにパッキングファクターにも優れている。このスポーク空洞の利点を生かしてERL 加速器を小型化し、LCS-γ/X線源を産業・学術分野への利用を図るため、\n超伝導スポーク空洞の開発を進めている。現在プレス加工したハーフスポークを使ってフルスポークにするための電子ビーム溶接試験を行っている。スポーク側面は複雑な曲線形状であり、さらにプレス成型による厚さ変化もあるため、溶接条件の最適化が重要である。溶接試験の現状について報告する。\n", "subitem_description_type": "Abstract"}]}, "item_access_right": {"attribute_name": "アクセス権", "attribute_value_mlt": [{"subitem_access_right": "metadata only access", "subitem_access_right_uri": "http://purl.org/coar/access_right/c_14cb"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "沢村, 勝"}], "nameIdentifiers": [{"nameIdentifier": "821815", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "羽島, 良一"}], "nameIdentifiers": [{"nameIdentifier": "821816", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "佐伯学行"}], "nameIdentifiers": [{"nameIdentifier": "821817", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "岩下芳久"}], "nameIdentifiers": [{"nameIdentifier": "821818", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "頓宮, 拓"}], "nameIdentifiers": [{"nameIdentifier": "821819", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "中村哲朗"}], "nameIdentifiers": [{"nameIdentifier": "821820", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "渡邉直久"}], "nameIdentifiers": [{"nameIdentifier": "821821", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Sawamura, Masaru", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "821822", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Hajima, Ryoichi", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "821823", "nameIdentifierScheme": "WEKO"}]}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "jpn"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "conference paper", "resourceuri": "http://purl.org/coar/resource_type/c_5794"}]}, "item_title": "超伝導スポーク空洞の電子ビーム溶接試験", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "超伝導スポーク空洞の電子ビーム溶接試験"}]}, "item_type_id": "10003", "owner": "1", "path": ["2"], "permalink_uri": "https://repo.qst.go.jp/records/77224", "pubdate": {"attribute_name": "公開日", "attribute_value": "2019-10-29"}, "publish_date": "2019-10-29", "publish_status": "0", "recid": "77224", "relation": {}, "relation_version_is_last": true, "title": ["超伝導スポーク空洞の電子ビーム溶接試験"], "weko_shared_id": -1}
超伝導スポーク空洞の電子ビーム溶接試験
https://repo.qst.go.jp/records/77224
https://repo.qst.go.jp/records/772242eef41cc-6fd5-4d6b-a3ce-732439c26243
Item type | 会議発表論文 / Conference Paper(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2019-10-29 | |||||
タイトル | ||||||
タイトル | 超伝導スポーク空洞の電子ビーム溶接試験 | |||||
言語 | ||||||
言語 | jpn | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_5794 | |||||
資源タイプ | conference paper | |||||
アクセス権 | ||||||
アクセス権 | metadata only access | |||||
アクセス権URI | http://purl.org/coar/access_right/c_14cb | |||||
著者 |
沢村, 勝
× 沢村, 勝× 羽島, 良一× 佐伯学行× 岩下芳久× 頓宮, 拓× 中村哲朗× 渡邉直久× Sawamura, Masaru× Hajima, Ryoichi |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | スポーク空洞は、周波数が同じならば楕円空洞よりサイズが小さく、さらにパッキングファクターにも優れている。このスポーク空洞の利点を生かしてERL 加速器を小型化し、LCS-γ/X線源を産業・学術分野への利用を図るため、 超伝導スポーク空洞の開発を進めている。現在プレス加工したハーフスポークを使ってフルスポークにするための電子ビーム溶接試験を行っている。スポーク側面は複雑な曲線形状であり、さらにプレス成型による厚さ変化もあるため、溶接条件の最適化が重要である。溶接試験の現状について報告する。 |
|||||
書誌情報 |
Proceedings of the 16th Annual Meeting of Particle Accelerator Society of Japan p. 709-711, 発行日 2019-10 |