Cleavage of the Graft Bonds in PVDF–g–St Films by Boiling Xylene Extraction and the Determination of the Molecular Weight of the Graft Chains

https://repo.qst.go.jp/records/76157
https://repo.qst.go.jp/records/76157
480dcd37-1b03-41d7-a2e1-dc9d59767464
Item type 学術雑誌論文 / Journal Article(1)
公開日 2019-07-01
タイトル
タイトル Cleavage of the Graft Bonds in PVDF–g–St Films by Boiling Xylene Extraction and the Determination of the Molecular Weight of the Graft Chains
言語
言語 eng
資源タイプ
資源タイプ識別子 http://purl.org/coar/resource_type/c_6501
資源タイプ journal article
アクセス権
アクセス権 metadata only access
アクセス権URI http://purl.org/coar/access_right/c_14cb
著者 Jinhua, Chen

× Jinhua, Chen

WEKO 799440

Jinhua, Chen

Search repository
Seko, Noriaki

× Seko, Noriaki

WEKO 799441

Seko, Noriaki

Search repository
Jinhua, Chen

× Jinhua, Chen

WEKO 799442

en Jinhua, Chen

Search repository
Seko, Noriaki

× Seko, Noriaki

WEKO 799443

en Seko, Noriaki

Search repository
抄録
内容記述タイプ Abstract
内容記述 To determine the molecular weight of graft chains in grafted films, the polystyrene graft chains of PVDF–g–St films synthesized by a pre-irradiation graft method are cleaved and separated by boiling xylene extraction. The analysis of the extracted material and the residual films by FTIR, nuclear magnetic resonance (NMR), and gel permeation chromatography (GPC) analyses indicates that most graft chains are removed from the PVDF–g–St films within 72 h of extraction time. Furthermore, the molecular weight of the residual films decreases quickly within 8 h of extraction and then remains virtually unchanged up to 72 h after extraction time. The degradation is due to the cleavage of graft bonds, which is mainly driven by the thermal degradation and the swelling of graft chains in solution. This allows determination of the molecular weight of graft chains by GPC analysis of the extracted material. The results indicate that the PVDF–g–St prepared in this study has the structure where one or two graft chains hang from each PVDF backbone.
書誌情報 polymers

巻 11, 号 7, p. 1098(1)-1098(17), 発行日 2019-07
出版者
出版者 MDPI
ISSN
収録物識別子タイプ ISSN
収録物識別子 2073-4360
DOI
識別子タイプ DOI
関連識別子 10.3390/polym11071098
関連サイト
識別子タイプ URI
関連識別子 https://www.mdpi.com/2073-4360/11/7/1098
戻る
0
views
See details
Views

Versions

Ver.1 2023-05-15 18:38:33.893844
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR 2.0
  • OAI-PMH JPCOAR 1.0
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3