In-bore laser welding tool for actively cooled divertor cassettes in JT-60SA

https://repo.qst.go.jp/records/85374
https://repo.qst.go.jp/records/85374
5131620c-3ce8-41c1-b840-183f9665339e
Item type 学術雑誌論文 / Journal Article(1)
公開日 2022-03-17
タイトル
タイトル In-bore laser welding tool for actively cooled divertor cassettes in JT-60SA
言語
言語 eng
資源タイプ
資源タイプ識別子 http://purl.org/coar/resource_type/c_6501
資源タイプ journal article
アクセス権
アクセス権 metadata only access
アクセス権URI http://purl.org/coar/access_right/c_14cb
著者 Takao, Hayashi

× Takao, Hayashi

WEKO 1055884

Takao, Hayashi

Search repository
Manabu, Takechi

× Manabu, Takechi

WEKO 1055885

Manabu, Takechi

Search repository
Go, Matsunaga

× Go, Matsunaga

WEKO 1055886

Go, Matsunaga

Search repository
Akihiko, Isayama

× Akihiko, Isayama

WEKO 1055887

Akihiko, Isayama

Search repository
Takao, Hayashi

× Takao, Hayashi

WEKO 1055888

en Takao, Hayashi

Search repository
Manabu, Takechi

× Manabu, Takechi

WEKO 1055889

en Manabu, Takechi

Search repository
Go, Matsunaga

× Go, Matsunaga

WEKO 1055890

en Go, Matsunaga

Search repository
Akihiko, Isayama

× Akihiko, Isayama

WEKO 1055891

en Akihiko, Isayama

Search repository
抄録
内容記述タイプ Abstract
内容記述 In-bore remote pipe welding tool has been upgraded for divertor cassettes of JT-60SA, where all plasma-facing components are actively cooled. Because the cooling pipes are surrounded by divertor cassette frame, pipe welding should be done from the inside of the pipe. The tool was equipped with a mirror to reflect the laser radially. Circumferential welding was performed by rotating the tool while injecting the laser. If fumes and spatters adhere to the laser reflecting mirror during welding, the laser will not reach the groove and the welding will not be stable. Upgrading the welding tool has realized to perform welding tests with a well-protected mirror and stable laser power. A misalignment between pipes at the groove is unavoidable in actual divertor cassettes of JT-60SA. The results of butt welding of short pipes indicated that it was possible not only in the gap but also in the combined state with angular and axial misalignment, covering a larger range than required by the actual cassette. It is notable that welding was possible even with an angular misalignment of 0.9◦ and an axial misalignment of 0.3 mm, where the maximum gap between pipes was about 0.9 mm.
書誌情報 Fusion Engineering and Design

巻 2022, 号 177, p. 113040, 発行日 2022-03
ISSN
収録物識別子タイプ ISSN
収録物識別子 0920-3796
DOI
識別子タイプ DOI
関連識別子 10.1016/j.fusengdes.2022.113040
関連サイト
識別子タイプ DOI
関連識別子 https://doi.org/10.1016/j.fusengdes.2022.113040
戻る
0
views
See details
Views

Versions

Ver.1 2023-05-15 16:46:57.057964
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR 2.0
  • OAI-PMH JPCOAR 1.0
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3