Evaluation of local residual strains in SiC/SiC composite and tungsten joints by synchrotron radiation

https://repo.qst.go.jp/records/72629
https://repo.qst.go.jp/records/72629
4492f31a-d46b-4739-9da3-e0d1195a8958
Item type 会議発表用資料 / Presentation(1)
公開日 2018-01-10
タイトル
タイトル Evaluation of local residual strains in SiC/SiC composite and tungsten joints by synchrotron radiation
言語
言語 jpn
資源タイプ
資源タイプ識別子 http://purl.org/coar/resource_type/c_c94f
資源タイプ conference object
アクセス権
アクセス権 metadata only access
アクセス権URI http://purl.org/coar/access_right/c_14cb
著者 安田, 良

× 安田, 良

WEKO 715356

安田, 良

Search repository
岸本, 弘達

× 岸本, 弘達

WEKO 715357

岸本, 弘達

Search repository
朝倉, 勇貴

× 朝倉, 勇貴

WEKO 715358

朝倉, 勇貴

Search repository
城, 鮎美

× 城, 鮎美

WEKO 715359

城, 鮎美

Search repository
菖蒲, 敬久

× 菖蒲, 敬久

WEKO 715360

菖蒲, 敬久

Search repository
安田 良

× 安田 良

WEKO 715361

en 安田 良

Search repository
城 鮎美

× 城 鮎美

WEKO 715362

en 城 鮎美

Search repository
抄録
内容記述タイプ Abstract
内容記述 Application of SiC/SiC composites and W metal joints to diverters is discussed for development of more attractive systems after DEMO reactors in future. Generally, the residual stress is caused near the interface of metal and ceramics joints by difference in the thermal expansion rate. It is considered that the residual stress lowered the integrity of the interface, so that control of the residual stress is very important to produce the good performance joints. To control the residual stress, knowledge on distribution of the residual stress is required. An X-ray diffraction residual stress measurement is an effective technique for obtaining distribution the residual stress nondestructively. In this work, we investigate the distribution of the residual stress in SiC/SiC composite and W metal sides using synchrotron radiation and discuss the influence of the residual stress on the integrity of the joints.
 A rectangular-shape-SiC/SiC composite and a W metal plate were prepared and joined by a hot press method at 1873K under compressive stress in Ar atmosphere. X –ray diffraction measurements were carried out at BL22XU in SPring-8. The joints sample was mounted on a stage on a multi-axis diffractometer installed in BL22XU to evaluate the residual strains by a strain-scanning method. X-ray energy in the experiments was 30 and 70 keV. The slit size determining a gauge volume is 30 by 30 m both incident and diffraction sides. The residual strains of SiC/SiC composites and W-metal are introduced from peak shift of (311) and (110), respectively.
From the results of the examinations, the drastically stress concentration region was not observed both SiC/SiC and W sides. Probably, it caused by small difference in the thermal expansion between W and SiC. In presentation we will report more detailed information.
会議概要(会議名, 開催地, 会期, 主催者等)
内容記述タイプ Other
内容記述 The 18th International Conference on Fusion Reactor Materials
発表年月日
日付 2017-11-09
日付タイプ Issued
戻る
0
views
See details
Views

Versions

Ver.1 2023-05-15 19:37:46.240842
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR 2.0
  • OAI-PMH JPCOAR 1.0
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3