Deuterium permeation behavior for damaged tungsten by ion implantation

https://repo.qst.go.jp/records/48289
https://repo.qst.go.jp/records/48289
e7db5e33-69d1-4782-a1a7-7c4d9a3b1b72
Item type 学術雑誌論文 / Journal Article(1)
公開日 2017-08-08
タイトル
タイトル Deuterium permeation behavior for damaged tungsten by ion implantation
言語
言語 eng
資源タイプ
資源タイプ識別子 http://purl.org/coar/resource_type/c_6501
資源タイプ journal article
アクセス権
アクセス権 metadata only access
アクセス権URI http://purl.org/coar/access_right/c_14cb
著者 Oya, Yasuhisa

× Oya, Yasuhisa

WEKO 485313

Oya, Yasuhisa

Search repository
Li, Xiaochun

× Li, Xiaochun

WEKO 485314

Li, Xiaochun

Search repository
Sato, Misaki

× Sato, Misaki

WEKO 485315

Sato, Misaki

Search repository
Yuyama, Kenta

× Yuyama, Kenta

WEKO 485316

Yuyama, Kenta

Search repository
Oyaidzu, Makoto

× Oyaidzu, Makoto

WEKO 485317

Oyaidzu, Makoto

Search repository
林, 巧

× 林, 巧

WEKO 485318

林, 巧

Search repository
山西, 敏彦

× 山西, 敏彦

WEKO 485319

山西, 敏彦

Search repository
Okuno, Kenji

× Okuno, Kenji

WEKO 485320

Okuno, Kenji

Search repository
小柳津 誠

× 小柳津 誠

WEKO 485321

en 小柳津 誠

Search repository
林 巧

× 林 巧

WEKO 485322

en 林 巧

Search repository
山西 敏彦

× 山西 敏彦

WEKO 485323

en 山西 敏彦

Search repository
抄録
内容記述タイプ Abstract
内容記述 The deuterium (D) permeation behaviors for ion-damaged tungsten (W) by 3 keV D-2 (+) and 10 keV C+ were studied. The D permeability was obtained for un-damaged W at various temperatures. For both D-2 (+) and C+ implanted W, the permeability was clearly reduced. But, for the D-2 (+) implanted W, the permeability was recovered by heating at 1173 K and it was almost consistent with that for un-damaged W. In the case of C+ implanted , the permeability was not recovered even if the sample was heated at 1173 K, indicating that the existence of carbon would prevent the recovery of permeation path in W. In addition, transmission electron microscope (TEM) observation showed the voids were grown by heating at 1173 K and not removed, showing the existence of damages would not largely influence on the hydrogen permeation behavior in W in the present study.
書誌情報 JOURNAL OF NUCLEAR SCIENCE AND TECHNOLOGY

巻 53, 号 3, p. 402-405, 発行日 2016-03
出版者
出版者 TAYLOR & FRAVCIS LTD.
ISSN
収録物識別子タイプ ISSN
収録物識別子 0022-3131
DOI
識別子タイプ DOI
関連識別子 10.1080/00223131.2015.1052583
戻る
0
views
See details
Views

Versions

Ver.1 2023-05-15 23:29:49.201512
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR 2.0
  • OAI-PMH JPCOAR 1.0
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3