{"_buckets": {"deposit": "160d6b48-4816-472c-8781-5f2836f6b062"}, "_deposit": {"created_by": 1, "id": "84931", "owners": [1], "pid": {"revision_id": 0, "type": "depid", "value": "84931"}, "status": "published"}, "_oai": {"id": "oai:repo.qst.go.jp:00084931", "sets": ["1"]}, "author_link": ["1024268", "1024275", "1024267", "1024271", "1024274", "1024265", "1024269", "1024264", "1024273", "1024266", "1024270", "1024272"], "item_8_biblio_info_7": {"attribute_name": "書誌情報", "attribute_value_mlt": [{"bibliographicIssueDates": {"bibliographicIssueDate": "2021-11", "bibliographicIssueDateType": "Issued"}, "bibliographicPageStart": "153422", "bibliographicVolumeNumber": "559", "bibliographic_titles": [{"bibliographic_title": "Journal of Nuclear Materials"}]}]}, "item_8_description_5": {"attribute_name": "抄録", "attribute_value_mlt": [{"subitem_description": "Characterization of the fuel debris has been required for decommissioning Fukushima Daiichi Nuclear Power Station. To understand the reaction mechanisms involved for mixed UO 2 –ZrO 2 compounds, these materials were treated at high temperatures (1473 to 1873 K) under oxidizing, inert, and reducing atmo- spheres. The reaction products were analysed by a combination of powder X-ray diffraction (PXRD) and X-ray absorption spectroscopic measurements of the U L III - and Zr K-edges. Principal component analysis of the X-ray absorption near edge structure and extended X-ray absorption fine structure of U L III - and Zr K-edges provided a breakdown of the composition of each species within the products, these results were further supported by PXRD. Under an oxidizing atmosphere, the formation of U 3 O 8 and U 2 Zr 5 O 15 was observed in equilibrium with UO 2 , monoclinic-ZrO 2 , and tetragonal-ZrO 2 . However, when O 2 gas was purged through the reaction tube during the cooling process to room temperature, pentavalent U in ZrU 2 O 7 was produced by the oxidation of solid solution UO 2 formed at \u003e 1774 K during the tempera- ture dropped at \u003c 1473 K. Under the inert atmosphere, mixed oxides of uranium were found to form at \u003e 1673 K due to a low concentration of O 2 impurity with the Ar gas. Although the oxidized UO 2 was able to form in such a system, tetravalent UO 2 and its solid solution were instead present throughout the whole temperature range examined under a reducing atmosphere (H 2 gas). This study can pave the way for understanding the interaction between the nuclear fuels and the cladding materials in damaged reactors enabling further simulation of possible decontamination procedures.", "subitem_description_type": "Abstract"}]}, "item_8_publisher_8": {"attribute_name": "出版者", "attribute_value_mlt": [{"subitem_publisher": "Elsevier"}]}, "item_8_relation_14": {"attribute_name": "DOI", "attribute_value_mlt": [{"subitem_relation_type_id": {"subitem_relation_type_id_text": "10.1016/j.jnucmat.2021.153422", "subitem_relation_type_select": "DOI"}}]}, "item_8_relation_17": {"attribute_name": "関連サイト", "attribute_value_mlt": [{"subitem_relation_type_id": {"subitem_relation_type_id_text": "https://www.sciencedirect.com/science/article/pii/S0022311521006425", "subitem_relation_type_select": "URI"}}]}, "item_8_source_id_9": {"attribute_name": "ISSN", "attribute_value_mlt": [{"subitem_source_identifier": "0022-3115", "subitem_source_identifier_type": "ISSN"}]}, "item_access_right": {"attribute_name": "アクセス権", "attribute_value_mlt": [{"subitem_access_right": "metadata only access", "subitem_access_right_uri": "http://purl.org/coar/access_right/c_14cb"}]}, "item_creator": {"attribute_name": "著者", "attribute_type": "creator", "attribute_value_mlt": [{"creatorNames": [{"creatorName": "Akihiro, Uehara"}], "nameIdentifiers": [{"nameIdentifier": "1024264", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Daisuke, Akiyama"}], "nameIdentifiers": [{"nameIdentifier": "1024265", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Ikeda-Ohno, Atsushi"}], "nameIdentifiers": [{"nameIdentifier": "1024266", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Chiya, Numako"}], "nameIdentifiers": [{"nameIdentifier": "1024267", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Yasuko, Terada"}], "nameIdentifiers": [{"nameIdentifier": "1024268", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Kiyofumi, Nitta"}], "nameIdentifiers": [{"nameIdentifier": "1024269", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Toshiaki, Ina"}], "nameIdentifiers": [{"nameIdentifier": "1024270", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Shino, Takeda"}], "nameIdentifiers": [{"nameIdentifier": "1024271", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Akira, Kirishima"}], "nameIdentifiers": [{"nameIdentifier": "1024272", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Nobuaki, Sato"}], "nameIdentifiers": [{"nameIdentifier": "1024273", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Akihiro, Uehara", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "1024274", "nameIdentifierScheme": "WEKO"}]}, {"creatorNames": [{"creatorName": "Shino, Takeda", "creatorNameLang": "en"}], "nameIdentifiers": [{"nameIdentifier": "1024275", "nameIdentifierScheme": "WEKO"}]}]}, "item_language": {"attribute_name": "言語", "attribute_value_mlt": [{"subitem_language": "eng"}]}, "item_resource_type": {"attribute_name": "資源タイプ", "attribute_value_mlt": [{"resourcetype": "journal article", "resourceuri": "http://purl.org/coar/resource_type/c_6501"}]}, "item_title": "Speciation on the reaction of uranium and zirconium oxides treated under oxidizing and reducing atmospheres", "item_titles": {"attribute_name": "タイトル", "attribute_value_mlt": [{"subitem_title": "Speciation on the reaction of uranium and zirconium oxides treated under oxidizing and reducing atmospheres"}]}, "item_type_id": "8", "owner": "1", "path": ["1"], "permalink_uri": "https://repo.qst.go.jp/records/84931", "pubdate": {"attribute_name": "公開日", "attribute_value": "2022-01-12"}, "publish_date": "2022-01-12", "publish_status": "0", "recid": "84931", "relation": {}, "relation_version_is_last": true, "title": ["Speciation on the reaction of uranium and zirconium oxides treated under oxidizing and reducing atmospheres"], "weko_shared_id": -1}
Speciation on the reaction of uranium and zirconium oxides treated under oxidizing and reducing atmospheres
https://repo.qst.go.jp/records/84931
https://repo.qst.go.jp/records/8493131274e4d-869f-48d3-8cdc-2b031310a82c
Item type | 学術雑誌論文 / Journal Article(1) | |||||
---|---|---|---|---|---|---|
公開日 | 2022-01-12 | |||||
タイトル | ||||||
タイトル | Speciation on the reaction of uranium and zirconium oxides treated under oxidizing and reducing atmospheres | |||||
言語 | ||||||
言語 | eng | |||||
資源タイプ | ||||||
資源タイプ識別子 | http://purl.org/coar/resource_type/c_6501 | |||||
資源タイプ | journal article | |||||
アクセス権 | ||||||
アクセス権 | metadata only access | |||||
アクセス権URI | http://purl.org/coar/access_right/c_14cb | |||||
著者 |
Akihiro, Uehara
× Akihiro, Uehara× Daisuke, Akiyama× Ikeda-Ohno, Atsushi× Chiya, Numako× Yasuko, Terada× Kiyofumi, Nitta× Toshiaki, Ina× Shino, Takeda× Akira, Kirishima× Nobuaki, Sato× Akihiro, Uehara× Shino, Takeda |
|||||
抄録 | ||||||
内容記述タイプ | Abstract | |||||
内容記述 | Characterization of the fuel debris has been required for decommissioning Fukushima Daiichi Nuclear Power Station. To understand the reaction mechanisms involved for mixed UO 2 –ZrO 2 compounds, these materials were treated at high temperatures (1473 to 1873 K) under oxidizing, inert, and reducing atmo- spheres. The reaction products were analysed by a combination of powder X-ray diffraction (PXRD) and X-ray absorption spectroscopic measurements of the U L III - and Zr K-edges. Principal component analysis of the X-ray absorption near edge structure and extended X-ray absorption fine structure of U L III - and Zr K-edges provided a breakdown of the composition of each species within the products, these results were further supported by PXRD. Under an oxidizing atmosphere, the formation of U 3 O 8 and U 2 Zr 5 O 15 was observed in equilibrium with UO 2 , monoclinic-ZrO 2 , and tetragonal-ZrO 2 . However, when O 2 gas was purged through the reaction tube during the cooling process to room temperature, pentavalent U in ZrU 2 O 7 was produced by the oxidation of solid solution UO 2 formed at > 1774 K during the tempera- ture dropped at < 1473 K. Under the inert atmosphere, mixed oxides of uranium were found to form at > 1673 K due to a low concentration of O 2 impurity with the Ar gas. Although the oxidized UO 2 was able to form in such a system, tetravalent UO 2 and its solid solution were instead present throughout the whole temperature range examined under a reducing atmosphere (H 2 gas). This study can pave the way for understanding the interaction between the nuclear fuels and the cladding materials in damaged reactors enabling further simulation of possible decontamination procedures. | |||||
書誌情報 |
Journal of Nuclear Materials 巻 559, p. 153422, 発行日 2021-11 |
|||||
出版者 | ||||||
出版者 | Elsevier | |||||
ISSN | ||||||
収録物識別子タイプ | ISSN | |||||
収録物識別子 | 0022-3115 | |||||
DOI | ||||||
識別子タイプ | DOI | |||||
関連識別子 | 10.1016/j.jnucmat.2021.153422 | |||||
関連サイト | ||||||
識別子タイプ | URI | |||||
関連識別子 | https://www.sciencedirect.com/science/article/pii/S0022311521006425 |