ログイン
言語:

WEKO3

  • トップ
  • ランキング
To
lat lon distance
To

Field does not validate



インデックスリンク

インデックスツリー

メールアドレスを入力してください。

WEKO

One fine body…

WEKO

One fine body…

アイテム

  1. 学会発表・講演等
  2. 口頭発表

Magnetically-guided liquid metal plasma-facing components

https://repo.qst.go.jp/records/66450
https://repo.qst.go.jp/records/66450
e258bcf8-3961-4cb9-8d76-df7986d0ca75
Item type 会議発表用資料 / Presentation(1)
公開日 2017-09-25
タイトル
タイトル Magnetically-guided liquid metal plasma-facing components
言語
言語 jpn
資源タイプ
資源タイプ識別子 http://purl.org/coar/resource_type/c_c94f
資源タイプ conference object
アクセス権
アクセス権 metadata only access
アクセス権URI http://purl.org/coar/access_right/c_14cb
著者 嶋田, 道也

× 嶋田, 道也

WEKO 653733

嶋田, 道也

Search repository
嶋田 道也

× 嶋田 道也

WEKO 653734

en 嶋田 道也

Search repository
抄録
内容記述タイプ Abstract
内容記述 In a strong magnetic field, liquid metal is frozen in the magnetic field. This property enables liquid metal to flow along the field line. In a divertor configuration with a lower single-null, a second separatrix exists above the plasma. Toroidally-continuous liquid metal sheets, poured through toroidal slots located above the plasma and radially outside the 2nd separatrix flux surface, move along the field line, absorbing heat and particles, reach the divertor at a glancing angle, and give toroidal momentum to the divertor liquid metal. This makes the divertor liquid metal rotate in the toroidal direction, making the temperature and particle content toroidally uniform. At the current quench in a disruption, toroidal current is induced automatically in the liquid metal surrounding the core plasma. The resultant jxB force pushes the liquid metal toward the core plasma, significantly mitigating the heat load and force on the first wall and the divertor. Use of magnetically-guided liquid metal PFC would also eliminate the need of fine toroidal alignment of the first wall and the divertor. The wall conditioning is done automatically during the discharge. Use of lithium-containing liquid metal (e.g. LiSn) would facilitate tritium breeding.
To avoid the complication due to the current induced in the liquid metal, the liquid metal sheets must be poured after the plasma current reaches a flat top and non-inductive current drive makes the one-turn voltage to a very low value. Current drive can be provided by ECW launched from above. Some diagnostics can be also installed on the upper port. Occasional interruption of the liquid metal flow would enable diagnosis from the midplane ports.
会議概要(会議名, 開催地, 会期, 主催者等)
内容記述タイプ Other
内容記述 「ダイバータの学理と応用」研究会
発表年月日
日付 2017-09-20
日付タイプ Issued
戻る
0
views
See details
Views

Versions

Ver.1 2023-05-15 20:48:48.860438
Show All versions

Share

Mendeley Twitter Facebook Print Addthis

Cite as

エクスポート

OAI-PMH
  • OAI-PMH JPCOAR 2.0
  • OAI-PMH JPCOAR 1.0
  • OAI-PMH DublinCore
  • OAI-PMH DDI
Other Formats
  • JSON
  • BIBTEX

Confirm


Powered by WEKO3


Powered by WEKO3